Phosphating is among the most widely used conversion treatments for steel. The wire surface is contacted with a phosphoric acid solution, and an insoluble, amorphous or crystalline film of metal phosphates forms on it. The film is non-electrolytic and forms by direct chemical reaction between metal and solution, with no external current. A crucial element is the conversion of a portion of the base metal, and this transformed component reacts far less to subsequent corrosion than the original surface. By giving the surface an equal potential, the film balances nearby cathodic and anodic galvanic sites, and the treatment is inexpensive and effective.
Where phosphating fits in steel surface processing
Chemical conversion coating techniques fall into three groups: phosphates, chromates and oxalates. Phosphates have replaced chromates because of their lower toxicity. Phosphating is the most common steel surface treatment, thanks to excellent adhesion, corrosion resistance, abrasion resistance and low cost.
Corrosion resistance depends on coating thickness, microstructure, surface treatment, density and coverage, and falls as porosity and cracking grow. Published studies have examined phosphating between 25 and 95 degrees Celsius. Two limitations come with the process: the bath sludge is hazardous and needs disposal, and the surface must be cleaned before coating, since contaminants cause poor adhesion.
Three main phosphate coating types
Three principal phosphate compounds are recognised in practice; the type depends on the end use.
- Fe3(PO4)2: suited to preparing metal surfaces before painting, with moderate corrosion resistance; a simpler route with less equipment and simpler wastewater treatment.
- Mn3(PO4)2: good absorbency onto the metal surface and good wear resistance; used in firearms and machinery requiring lubrication. Preferred over Fe3(PO4)2.
- Zn3(PO4)2: excellent corrosion and wear resistance, good lubrication and affordable application; used extensively in industry and gives a good substrate for metallic painting.
Chemistry of the zinc phosphate bath
All phosphating baths are based on a diluted H3PO4 solution with one or more alkali metal or heavy metal ions, and consist mainly of primary metal phosphates plus free H3PO4. Free phosphoric acid prompts dissolution of iron at the microanodes, while hydrogen evolution takes place at the microcathodic sites. The change in pH shifts the hydrolytic equilibrium between soluble primary and insoluble tertiary phosphates, so the heavy metal tertiary phosphates are transformed and deposited, and the iron phosphate leaves as sludge.
- Diluted H3PO4: regulates the free acid and total acid values, which relate to the concentrations of free and total phosphates in the solution respectively.
- Accelerators: reduce coating time, which ranges from seconds to hours. Oxidizing agents such as NO3- and NO2- affect the depolarization of the hydrogen evolution reaction by consuming hydrogen ions at cathodic sites. Adding nitrate, nitride and chlorate speeds up coating formation.
- Activators: excellent phosphating requires the etching rate of the substrate to be substantially lower than the coating formation rate. Fluorides are the usual activators in Zn3(PO4)2 solutions.
- Coating agents: the coating consists mainly of hopeite, used to prevent corrosion of steel, Al alloys and Mn alloys. Its nontoxic and anticorrosive qualities make it a substitute for Cr conversion coating.
- Other agents: organic acids combine with some insoluble phosphates to produce a soluble complex that stabilises the bath. Additives such as Ni, Mg, Ca and Mn, and compounds such as Ni2+, Mn2+, Mo2+ and Ca2+, raise adhesion and corrosion resistance.
The phosphating line, step by step
Poor surface preparation is the most common cause of coating failure; the flow can be modified with pre- or post-processing stages.
- Polishing: the metal is polished with emery paper of various grades for smoothness and to remove rust.
- Alkaline degreasing: elimination of grease, dust, rust and metal filings before the chemical film forms; preferably in a NaOH solution, or by brushing or blasting.
- Rinsing: preferably in deionized water and alcohol, so alkaline residue does not contaminate the phosphating step.
- Acid pickling: HCl, H2SO4 and H3PO4 remove mill scale and rust; with inhibitors, diluted 5 to 10 wt% H2SO4 and HCl remove inorganic pollutants by converting them to ferrous salts.
- Second rinsing: removes acid carried over from pickling; HCl drag-in causes uneven coatings and harder bath control.
- Activation: creates tiny active crystal centres on the surface for a uniform coating; acidic or alkaline activation is used.
- Phosphating: spray or immersion is used for ferrous and non-ferrous metals, at 30 to 99 degrees Celsius and 30 seconds to 6 hours.
- Third rinsing and drying: deionized water removes soluble salts, acid residues and non-adherent particles that encourage blistering of the paint coatings; warm air fans and blow offs are the cheapest drying methods.
Quality control and coating characterisation
In industry, coating thickness is reported as weight per unit area, typically g/m2 or mg/ft2, called coating weight, because thickness measurement is hard on uneven substrates. Coatings range from 1 to 50 microns. Coating weight follows W = (W1 – W2) / S, with W the coating weight in g/m2, S the substrate area in m2, and W1 and W2 the sample weights after and before phosphating.
- Porosity: porosity decreases as coating thickness rises, and depends on the phosphate solution, treatment length, Fe content of the bath and coating composition.
- Structure and composition: energy-dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) are typically used to examine the structure and chemical makeup of Zn3(PO4)2 coatings, and XRD shows hopeite makes up most of them. Other reported techniques include electron spin resonance and scanning electron microscopy.
Adsorption, thermodynamics and the link to wire drawing
Adsorption is the buildup of molecular species onto a solid surface, and an isotherm expresses the equilibrium relationship between fluid concentration and the amount adsorbed at constant temperature. To model an isotherm, static adsorption tests are run on the liquid-solid interface at various concentrations. The Langmuir isotherm describes a homogeneous monolayer and the Freundlich isotherm multilayer adsorption on a heterogeneous surface; Henry and Redlich-Peterson isotherms also exist.
- Thermodynamic parameters: the adsorption constant Kads, the change in entropy, the change in Gibbs free energy and the adsorption enthalpy are computed from the relevant equations, where R is the gas constant (8.314 J/mol/K) and T the absolute temperature. Negative Gibbs free energy indicates spontaneous adsorption, positive enthalpy an endothermic process, negative entropy decreasing randomness.
- Mass transfer coefficient: the mass transfer coefficient kf, in kg/m2/s, reveals how much coating material is adsorbed onto a given area of metal in a given time, and assesses coating performance.
- Industrial applications: corrosion control, especially with polymer films; paint and other organic coatings; help in cold forming of steel such as wire drawing; improved friction characteristics including friction coefficient, wear resistance, break-in and anti-galling; and resistance to wetting by molten metal.
Source: Portugaliae Electrochimica Acta